Take 30% Off All Dyes For A Limited Time
These professional quality anodizing dyes
provide consistent, quality results. The same dyes are
sold to professional anodizing shops all over the world.
Each 4oz bottle of dye concentrate makes 2 Gallons.
|
|
Each anodizing kit is supplied
with a color wheel. Dyes can be mixed together to
create a host of different colors. The dyes are
in concentrated liquid form, a 4oz bottle makes
up 2 gals of ready to use dye. To make up different
colors, we suggest that you make up the colors to
the correct dilution first, then take a quantity
of each dye and blend them together. |
These colors are approximate. The finish
will normally have a more 'metallic' look, and will
vary slightly depending on the alloy and surface preparation.
Procedure for Obtaining
Dyed Anodize
Anodize the aluminum at 60-75°F for 90 minutes
at 4.5 amps per sq foot or 0.03 amps per sq inch. Use
our Anodizing Kit.
After thorough rinsing, immerse the part in the dye
at a temperature of 140°F for 15 minutes.
Finally, seal by hanging the part in a sealer bath
for 15 minutes.
Note: All dyes are suitable for high temp and low temp
sealants, except Grey BL and Yellow 4A, which should
not be sealed using LT Sealer.
|