Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > Powder Coating Supplies > Powder Coating System
Search Caswell Inc.

Web Site Features
Start Here

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

Powder Coating System

 

Powder Coating System

JUST LIKE THE PROFESSIONALS!

NOW AVAILABLE - HIGH VOLTAGE 50KV SYSTEM - UNDER $230.00. READ MORE HERE

Powder Coating System

Here is a great way to paint small parts. The process is simple, requiring only an old electric oven to bake the finish on.

Here’s how it works!

Firstly, the surface of the part is suitably prepared, just as you would for any other paint job.

Applications Of This Product
  • Paint a durable layer, quickly and evenly onto any part.

Sample Work Completed With This Product

Powder Coating Gallery


You Must Supply

Curing Lamp or Dedicated Electric Oven

Air Compressor


Related Products


The special gun is attached to an air compressor, and a power unit. The air blows the powder from the gun, and the power unit gives the powder a positive charge. At the same time, the power unit is connected to the piece being coated, and so it has a negative charge. As the positive paint particles fly through the air, they are attracted to the part and lay in an even layer over the entire area of the part. (This works a little like dust on a TV screen.)

The part is then placed in an dedicated electric oven, and baked for a while. This cures the coating to a tough chemical resistant finish.

It is important not to use a gas oven, as the emissions from the coating are flammable.

The moisture filter must be changed regularly to ensure best operation.

Why are our powder guns better than our competitors?

  • Our powders cups are tapered to provide smoother flow.
  • The charge switch is controlled by a foot pedal, leaving your hands free - competitor's are hand controlled.
  • The power pack is more compact and lighter.
  • Sturdier construction - less powder leaks
  • Works with any manufacturers virgin powder coating. Do not use reclaimed powder.

Now Includes 1 Pound Of Super Wet Black Powder Coating

Super Wet Black On Alternator
Courtesy myillwillinc

  • 30 Day Limited Warranty
  • Input Voltage: 110volt 60HZ AC
  • Air Requirement: 15PSI @ 5 CFM
  • Fixed Output Voltage: 16KVDC 
  • Manual Discharge 
  • 2 x Powder Gun Cups
  • 3 x Conical Fan Spray Pattern tips
  • External High Voltage Power Supply
  • In line disposable filter
  • Foot switch
  • Ground Clip Cable
  • Free Technical Support
  • 1 lb Super Wet Black Powder Coating
Powder Coating Gun

We Now Sell Over 100 Different Powder Coating Colors

Resources:

Quantity Product Code Name Price  
PCGUN125 Powder Coating System $95.00
Not Hazardous
PCCUP Powder Coating Gun Cup $2.99
Not Hazardous
PCFILTER Disposable Moisture Filter $5.00
Not Hazardous
     
     
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
  * - Other minor household items may be required, such as gloves, dust mask etc.
Login or Email
Password
Lost Password?
Create An Account